Multi-Criteria Performance Analysis of Dry, Vortex Air and Compressed Air Environments in Turning Hastelloy X Superalloy
Gazi Mühendislik Bilimleri Dergisi, vol.11, no.2, pp.243-253, 2025 (TRDizin)
- Publication Type: Article / Article
- Volume: 11 Issue: 2
- Publication Date: 2025
- Doi Number: 10.30855/gmbd.070525a07
- Journal Name: Gazi Mühendislik Bilimleri Dergisi
- Journal Indexes: TR DİZİN (ULAKBİM)
- Page Numbers: pp.243-253
- Hacettepe University Affiliated: Yes